BRICK

BRICK

 

 

FIRE BRICK

img1.gif

Item

SK-34

SK-36

SK-38

SK-40

Maximum Operating Temperature (℃)

1350

1450

1550

1700

Apparent Porosity(%)

24

25

24

19

Bulk Density(g/㎤)

2.1

2.25

2.4

2.85

Cold Crushing Strength(kg/㎠)

200

250

300

700

 

 

 

INSULATING BRICK

img7.gif

Item

B-1

B-2

B-3

B-5

Temp. (℃)
Reheating Shrinkage less than 2%

900

1,000

1,100

1,300

Bulk Density(g/㎤)

0.70≥

0.70≥

0.75≥

0.80≥

Cold Crushing Strength(kg/㎠)

25≤

25≤

25≤

25≤

Thermal Conductivity(kcal/mh℃)

0.17≥

0.18≥

0.18≥

0.23≥

 

 

 

IMPORT HIGH TEMPERATURE FIRE BRICK

img9.gif

Item

MIZZOU DV GREENAL-90 GREENAL-94

Maximum Operating Temperature(℃)

1820

1650

1650

1800

Manufacturer

A.P.GREEN

 

 

 

IMPORT INSULATING FIRE BRICK

img5.gif

Item

BNZ-23

BNZ-26

BNZ-28

BNZ-30

Maximum Operating Temperature(℃)

1260

1427

1538

1649

manufacturer

BNZ MATERIALS,INC.

 

 

 

IMPORT HIGH TEMPERATURE BONDING MORTAR

img6.gif

Back-up due to the impact of foreign matter or dust from the GAS on high intensity mixed Mortar joints of adhesive chemical re-Steel Casing corrosion, erosion, and to prevent
  the adhesive strength even at high temperatures, higher than the strength of the brick itself . Mortar Joints strength robust bonding by high brick structure has.


Imports:Sairset,Blackbond